Hi again everyone: I want to thank you all for your advice. The consensus is that I have my new embedding center's cold plate set way too low at -14C, and that I should try raising it to around -5C to cure my cracked block problem. I will run some test blocks over the weekend, and then embed them at this new temperature on Monday. Otherwise my Valida embedding center is working very nicely (as did the HistoStar when I demoed it). The cassette holding tank can accommodate a large number of brain specimens and the controls are very easy to use. Thanks again for your advice. Have a great weekend.
Tim Tim Wheelock Harvard Brain Bank McLean Hospital Belmont, MA The information in this e-mail is intended only for the person to whom it is addressed. If you believe this e-mail was sent to you in error and the e-mail contains patient information, please contact the Partners Compliance HelpLine at http://www.partners.org/complianceline . If the e-mail was sent to you in error but does not contain patient information, please contact the sender and properly dispose of the e-mail. _______________________________________________ Histonet mailing list Histonet@lists.utsouthwestern.edu http://lists.utsouthwestern.edu/mailman/listinfo/histonet