0.7% Formic Acid for 30 seconds with sonication, then rinse well in DI water.
Jack
On Aug 19, 2010, at 2:22 PM, "Herrick, James L. (Jim)"
wrote:
> Good afternoon everybody,
>
> Would anyone be willing to offer their wisdom on the best etching
> solution for 50 to 75 micron thick jaw specimens
Good afternoon everybody,
Would anyone be willing to offer their wisdom on the best etching
solution for 50 to 75 micron thick jaw specimens embedded in MMA? The
stain we want to use is a Trichrome. Thanks in advance for your help.
Jim
___