Hello everyone,
 
I was asked to find out how to dry slides quickly.  They are glass coverslipped 
in an automated coverslipper at the reference lab we use and the our docs want 
them filed in less than 12 hours from the time they are coverslipped.   We have 
been putting them in a 125 degree C convection oven for a few hours but the 
slides still get all stuck together in the file.  They will not consider film 
coverslipping. 
 
Does anyone else file this quickly?  I am grateful for any suggestions!
 
Erin Martin UCSF Dermatopathology