Peggy,  If your microtome will hold a sharp D profile or a tungsten carbide 
blade,  you might be able to get consistent sections.  I find that EDTA 
decalcification hardens the tissue ( as if it wasn't hard enough already).  
Also, extending the times for the paraffin infiltration is helpful and soaking 
the block in icy/soapy detergent in the freezer works on some samples.

~ VIcki