I was wondering if you could help me with my MMA formulation.  I have been 
using a formulation that I found in a published paper.  My current embedding 
formulation is 80ml MMA, 20ml Dibutyl Phthalate and 3g Benzoyl Peroxide.  The 
samples are embedded after three days of infiltration, one change per day, with 
the formulation of 80ml MMA and 20ml Dibutyl Phthalate. Lately have noticed 
that there is a pressure build up in the vials.  I have had a few vials burst 
almost immediately once placed in the heated waterbath. I am filling the glass 
vials full with the embedding solution, capping them and then placing them in a 
water bath in a 37 degree oven.  They are completely polymerized by the next 
morning. I am also getting bubbles in the plastic when polymerized.

I have two questions: Is there any way to get rid of the bubbles in the plastic 
and of more concern what do you think is causing the pressure build up?

I would really appreciate any help that you can provide.

Thank you,
Nikki