0.7% Formic Acid for 30 seconds with sonication, then rinse well in DI water.
Jack On Aug 19, 2010, at 2:22 PM, "Herrick, James L. (Jim)" <herrick.ja...@mayo.edu> wrote: > Good afternoon everybody, > > Would anyone be willing to offer their wisdom on the best etching > solution for 50 to 75 micron thick jaw specimens embedded in MMA? The > stain we want to use is a Trichrome. Thanks in advance for your help. > > Jim > > > _______________________________________________ > Histonet mailing list > Histonet@lists.utsouthwestern.edu > http://lists.utsouthwestern.edu/mailman/listinfo/histonet > _______________________________________________ Histonet mailing list Histonet@lists.utsouthwestern.edu http://lists.utsouthwestern.edu/mailman/listinfo/histonet