Dear community,
I'm struggling with the data analysis of some Co samples, i think it
might be some cobalt carbide. I was wondering if someone would be
willing to share the spectrum of the Co2C reference please? That would
be very helpful.
Thank you in advance!
Cheers,
Antonio Aguilar
--
Postdoctoral fellow
Beamlines CRG FAME (BM30B) & FAME-UHD (BM16) | ESRF
ESRF - The European Synchrotron
71 Avenue des Martyrs, 38043 Grenoble, France
Tel: +33 (0)4 76 88 25 46 - Bureau : LOB 2-50