Dear Valentijn,
for cementite (Fe3C), we have some high resolution data in our database (HERFD XAS and K-beta XES):
https://www.sshade.eu/data/EXPERIMENT_SOC_20181115_002

Cheers
Denis

Le 15/11/2021 à 10:10, Valentijn De Coster a écrit :

Dear ifeffit mailing list,

My name is Valentijn De Coster. I am a PhD student at Ghent University, Belgium, working on Ni and Fe materials for CO2 utilization.

I am currently looking for Fe and Ni carbide (Fe3C, Ni3C) reference XAS spectra, at the respective Fe K and Ni K edges, for fingerprinting purposes. As such, I was wondering whether anyone would have such data available.

On a side note, I checked the CARS database, and while this has an Fe3C (Fe K edge) reference, the data file does not contain the Energy values of the spectrum.

Thank you in advance for your time.

Kind regards,

Valentijn De Coster

Image result for ghent university logo**

        

*Valentijn De Coster*

*PhD Student*

*Laboratory for Chemical Technology (LCT) *

Department of Materials, Textiles and Chemical Engineering**

Technologiepark 125, 9052 Ghent, Belgium

T: +32 9 331 17 M: +32 (0) 331 17 10

https://www.lct.ugent.be <https://www.lct.ugent.be/> https://helpdesk.UGent.be/e-maildisclaimer.php <https://helpdesk.ugent.be/e-maildisclaimer.php>

Member of CSC: https://www.csc.ugent.be <https://www.csc.ugent.be/>


_______________________________________________
Ifeffit mailing list
Ifeffit@millenia.cars.aps.anl.gov
http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit

--
Institut Néel - CNRS
FAME/FAME-UHD beamlines - ESRF
+33 476 881 045

_______________________________________________
Ifeffit mailing list
Ifeffit@millenia.cars.aps.anl.gov
http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit

Reply via email to