It definitely comes as normalized, Mark.

Thanks for the advice.

Serge Vidal
KR2 "Kilimanjaro Cloud"
Paris, France





"Mark Langford" <[email protected]>

Envoyé par : [email protected]
2005-06-07 00:19
Veuillez répondre à KRnet
Remis le : 2005-06-07 00:14


        Pour :  "KRnet" <[email protected]>
        cc :    (ccc : Serge VIDAL/DNSA/SAGEM)
        Objet : Re: KR> 4130 steel



Serge wrote:

> >If I buy strips of 4130 steel of the correct thickness from Aircraft
> >Spruce, can I use them as they are to make WAFs, or is there any
> >treatment (other that surface treatment) that I must apply?

The heat treatment is "condition N".  You can either start there or end
there, but that's the way it needs to be when you're finished.  I think 
when
you buy it from AS&S, that's the way it is, but I'd check to make sure.

Mark Langford, Huntsville, Alabama
see KR2S project N56ML at http://home.hiwaay.net/~langford
email to N56ML "at" hiwaay.net
--------------------------------------------------------------


_______________________________________
Search the KRnet Archives at http://www.maddyhome.com/krsrch/index.jsp
to UNsubscribe from KRnet, send a message to [email protected]
please see other KRnet info at http://www.krnet.org/info.html


Reply via email to