When heat treating, pre heat an electric oven to about 450 deg. F. use an
magnet held in one hand and heat the part up with an acetylene torch until
the part becomes non magnetic. Put it into the oven and turn it off. Let it
cool gradually.

-Joe


Message: 7
List-Post: [email protected]
Date: Tue, 7 Jun 2005 00:27:08 -0400
From: "Brian Kraut" <[email protected]>
Subject: RE: KR> 4130 steel
To: "KRnet" <[email protected]>
Message-ID: <[email protected]>
Content-Type: text/plain;       charset="us-ascii"

I am not an expert on this, but I believe that you heat to a dull red to
normalize.