I work fiberglass in the winter at temps 60 to 70 deg F using heat lamps to
promote curing, hot air gun to spread resin and saturate cloth. The curing
times are slower but it works. I intend to post curing in the summer sun to
being the planes surface to 140 deg F. using black plastic sheathing.
Most of the work has been around 6 to 10 sq. ft.
KRron 
http://www.jrl-engineering.com 
Our Attitude Makes The Difference!

-----Original Message-----
From: krnet-boun...@mylist.net [mailto:krnet-boun...@mylist.net] On Behalf
Of Jack Cooper
Sent: Tuesday, November 29, 2005 11:44 AM
To: KRnet
Subject: RE: KR> Temps for glass work

I have done small areas of glass work in the winter and used halogen lamps
to keep the area warm.

Jack Cooper


> [Original Message]
> From: Pitts Eric MSgt 181FW/MXOO <eric.pi...@interr.ang.af.mil>
> To: <kr...@mylist.net>
> Date: 11/29/2005 10:39:51 AM
> Subject: KR> Temps for glass work
>
> What would be the normal range of temps for doing glass lay ups. I will
have
> my garage heated this winter and am wanting to do some glass work.
>  
> Eric Pitts
> Terre Haute IN
> KR2S
> http://home.att.net/~e.j.pitts/ <http://home.att.net/~e.j.pitts/> 
>
>   
>
>  
> _______________________________________
> Search the KRnet Archives at http://www.maddyhome.com/krsrch/index.jsp
> to UNsubscribe from KRnet, send a message to krnet-le...@mylist.net
> please see other KRnet info at http://www.krnet.org/info.html




_______________________________________
Search the KRnet Archives at http://www.maddyhome.com/krsrch/index.jsp
to UNsubscribe from KRnet, send a message to krnet-le...@mylist.net
please see other KRnet info at http://www.krnet.org/info.html




Reply via email to