I have been using Dap 00204 Plastic Resin Glue.  Same issues with temp and 
clamping you indicated so I don't think it's any better or worse.  I will use 
T88 for little bit of the structural stuff I have left to do.

Craig
www.kr2seafury.com
Corvair 2780cc

--- On Thu, 8/18/11, Patrick and Robin Russo <patru...@myfairpoint.net> wrote:

> From: Patrick and Robin Russo <patru...@myfairpoint.net>
> Subject: Re: KR> Resorcinol Glue
> To: "KRnet" <kr...@mylist.net>
> Date: Thursday, August 18, 2011, 4:17 PM
> I have 50 years of woodworking
> experience and have always been less than 
> pleased with Resorcinal glues. If it's not clamping
> pressure then it is 
> consistency, working time, shop temperature, shelf life,
> etc.,etc. It is not 
> a forgiving glue. Alternatives...??? T-88..??? difficult to
> do larges 
> assemblies, good gap filler but if its filling a gap you
> have a bad 
> (brittle) joint, also need more than moderate clamping
> pressure.  