I am by no means the expert on this, so I hope others will weigh in . . . But 
I'll
repeat what I know, and hopefully get it right . . .

Rubbing compound is a mild abrasive suspended in a paste, a paste much like 
liquid
wax for a car, and is a safe way to take the oxidation out of gelcoat . . . It 
comes
in degrees of abrasiveness and is available at marine outlets . . . It can be 
applied
with an orbital polisher, but one should take care not to use too much pressure 
and
"burn" the gelcoat, which I believe will yellow when damaged by heat.

Penetrol, and I'm not sure of the spelling, is a paint additive . . . I think 
for
enamel paint . . . I believe it's a solvent, but someone please correct me if 
I'm
wrong . . . I believe it is available as "Marine Penetrol", but I've used the 
stuff
available at any hardware store . . . It is applied, left very briefly, and 
wiped
off, leaving a rich shine in the gelcoat . . . It's most impressive use I've 
seen is
Larry Yake's yellow-hulled M17, Tullamore . . .

Vertglass was one brand of miracle fiberglass restorer . . . I don't know if 
it's
available anymore . . . Poliglow is another brand, one, I believe, that 
received high
marks from Practical Sailor magazine.  I'm not sure what the miracle restorers 
do, if
they're like rubbing compound and wax in one or what, but Poliglow would 
basically
used to preserve the gelcoat's finish, like wax . . . I think . . . Please 
correct me
if I'm wrong . . . I believe these miracle restorers tout that they can be used 
on
oxidized gelcoat, skip the rubbing compound, and produce good results, but we 
had
much better success with Vertglass after using rubbing compound first . . .

These are three steps I'm considering, but there's more than one way to skin 
this
cat, and West Marine sells complete kits for gelcoat care . . . I think Star 
Bright
caries a variation of every gelcoat, metal and wood preservative/restorer 
conceivable
. . .

All the products make magnificent claims . . .

But I saw pics of Tod's Busca after the Poliglow, don't know what steps he used
before, and it was very impressive . . .

----- Original Message ----- 
From: Rick Langer
To: [email protected]
Sent: Tuesday, January 25, 2005 9:54 AM
Subject: i was thinkin' . . . too

Craig,

My blue hull is oxidized too and I'd like to bring it back.  I have a 9"
compounder and a Cyclo random orbital polisher which I've used to polish a
vintage Airstream trailer.  I'm guessing that polishing fiberglass is a lot
easier than aluminum, but I'm a bit confused i.e.  rubbing compound,
Penetrol(?), Poliglow, Vertglass.

I wonder if you could give us a brief tutorial on bringing back and keeping
the shine on our boats?

BTW, my boat has repaired gouges, but the color match is so bad that I wish
they were left alone.  I went through a similar thing when polishing my
Airstream.  The experts advised me to leave the gouges and large scratches
alone and just polish them, kind of adds character.  I think they were
right.

Thanks,
Rick Langer
M15 #337

 Date: Mon, 24 Jan 2005 23:29:50 -0500
 From: "Craig F. Honshell" <[EMAIL PROTECTED]>
 Subject: M_Boats: i was thinkin' . . .
 To: "For and about Montgomery Sailboats"
 <[email protected]>
 Message-ID: <[EMAIL PROTECTED]>
 Content-Type: text/plain; charset="iso-8859-1"

 . . . this spring that I'd like to buff out my hull's oxidation, then go
over it
 completely with Penetrol, then finish it with Poliglow or comparable
miracle
 restorative . . . I think we used "Vertglass", something like that, on the
Flicka one
 year . . . Don't know if that stuff is still available . . .

 I have gouges in my shear stripe that aren't going to go away without
major
 restoration, but perhaps I can draw the eye away from them with a really
shiny hull .
 . .  :-)




_______________________________________________
http://mailman.xmission.com/cgi-bin/mailman/listinfo/montgomery_boats
_______________________________________________
http://mailman.xmission.com/cgi-bin/mailman/listinfo/montgomery_boats

Reply via email to