There is a guy on the Tartan 27 web site that has been using a two stage vacuum 
pump to dry out his deck core and keel.  He claims to be able to pull a vacuum 
so strong that he can boil water with an ambient temperature below 50 degrees 
F.  His user name is "cstroup".  He has posted under both the "Discussion" and 
"Projects" forums.  He uses several descant filters and a "cold filter" with 
dry ice to condense out the extracted moisture.  This guy has really given some 
thought to the process.

I have no idea how much a two stage pump costs, but the concept of drilling a 
hole to suck the water out and then pump resin back in sure sound appealing to 
me.  

http://www.tartan27owners.com/discussion.htm

OT along these lines - I have a section of sill plate in my detached garage 
that has wood rot.  The outer third is soft, the inner is solid.  Also the tail 
ends of some rafters are "slightly" rotten.  The garage did not have any 
ventilation and a PO planted several trees too close.  We have cut down the 
trees and replaced most of the old siding with plywood.  We will install new 
siding and soffits.  I am hung up on dealing with this sill with the rot.  I am 
think of using a penetrating epoxy from www.rotdoctor.com or Git Rot.  Please 
contact me off list if you have any suggestions as to whether this is a good or 
bad idea.