Dennis,
        no I didn't mean 1 oz. foil or starting copper weight, I meant 1 oz.
plating. I thought that my comment was fairly clear but I guess not. I had
also mentioned that they have an automated plating line which supposedly was
their reason for only plating one weight of copper without screwing up their
line for varying plating thickness.
        As I mentioned, Daniel says he has had different experiences with
Enigma, so now I am in the dark about why we were told they only plated 1
oz. Cu.

Sincerely,
Brad Velander.

Lead PCB Designer
Norsat International Inc.
Microwave Products
Tel   (604) 292-9089 (direct line)
Fax  (604) 292-9010
email: [EMAIL PROTECTED]
http://www.norsat.com


-----Original Message-----
From: Dennis Saputelli [mailto:[EMAIL PROTECTED]]
Sent: Monday, July 29, 2002 6:13 PM
To: Protel EDA Forum
Subject: Re: [PEDA] PCB houses


just to clarify terms here
don't you really mean 'starting weight' 1oz copper not '1 oz plating'?

1/2 oz starting wt is used for finer pitch and lines and 2 oz for some
power applications

the traditional tin lead plating is in addition to that

Dennis Saputelli


************************************************************************
* Tracking #: A8C2DED5D263AB418172C67F406A6727ECE3176F
*
************************************************************************

* * * * * * * * * * * * * * * * * * * * * * * * * * * * * *
* To post a message: mailto:[EMAIL PROTECTED]
*
* To leave this list visit:
* http://www.techservinc.com/protelusers/leave.html
*
* Contact the list manager:
* mailto:[EMAIL PROTECTED]
*
* Forum Guidelines Rules:
* http://www.techservinc.com/protelusers/forumrules.html
*
* Browse or Search previous postings:
* http://www.mail-archive.com/proteledaforum@techservinc.com
* * * * * * * * * * * * * * * * * * * * * * * * * * * * * *

Reply via email to