x y z B
Zr 0 0 0 1.66
O 0 .5 .185 3.11
a 3.64
b 3.64
c 5.27
Bruce A. Hudgens
Research Associate
USG Research & Technical Center
700 N Hwy 45
Libertyville, IL 60048
[EMAIL PROTECTED]
(847) 970-5064 Voice
(847) 362-4871 Fax
> -----Original Message-----
> From: Jack Badenhorst [SMTP:[EMAIL PROTECTED]]
> Sent: Friday, October 30, 1998 8:23 AM
> To: [EMAIL PROTECTED]
> Subject: Zirconium oxide
>
> Hi everyone
> I need some help with the atomic positions for the following Zirconium
> Oxides.
> 1. Tetragonal (24-1164 , 42-1164, 17-0923) and
> 2. the cubic form
> Can anyone help me?
> Thanks
> Regards Jack