On Thu, 9 Mar 2000, Armel Le Bail wrote:

> >I have added the possibility to handle Learnt Profiles to the BGMN &
> >related programs suite. Actual level is now 3.0.0. Usability was
> >extended to Jun 30 2000. See www.bgmn.de or any of the IUCR CCP14 mirrors.
> 
> This is far from the so-called FP (Fundamental Parameter) approach.
> But I agree that it is best ;-) as said in a paper at the 1998 Denver
> X-ray Conference : http://sdpd.univ-lemans.fr/microstruct/denver/
 
I would prefer the BGMN FP method whenever possible. As we know,
there are diffractometer set-ups which cannot be handled by our FP method.
For handling the latter, we have introduced our variant of learnt
profiles.

Our learnt profiles method is more near to the FP method than other
learnt profiles: We extract the pure geometric part from the
standard profiles. This work is done by the VERZERR programm. These
geometric data are parametrized and handled equivalent to the FP geometric
data.

Indeed, VERZERR is a very old program. Firstly, I have described
it in my doctoral thesis dating back to 1984 (which is now set online).

>From 1982 to 1992, I have tried to introduce learnt profiles to
the practice in routine labs. This has failed strongly for several
times. The amount of measuring time, which we need for calibration,
is about one week. This is mostly inacceptable in a routine lab.

Therefore, I have started developing my raytracing FP method in 1993.
Using up-to-date tube tails correction, it gives more accurate profiles
compared to learnt profiles. Plus, the measuring time for the tube tails
is about half an hour! This is much less compared to learnt profiles.
Therefore, I recommend our FP method whenever possible.

We will have a poster at EPDIC 7 comparing both methods within BGMN.
As I hope, there will be an intensive discussion.

> 
> There are at least 2 ways already developed for the Learnt Profiles
> approach : those used in XRS-82 and in ARIT-83 (Fourier coefficients +
> special angular variation law) Rietveld programs.
> 
> What is proposed exactly in BGMN ?

We do not use Fourier coefficients or Fourier deconvolution. We use
the method of describing the geometric part as expansion into squared
Lorentzian functions, which is identic to the FP parametrization.

Sincerely yours

J"org Bergmann
Dresden
[EMAIL PROTECTED]


Reply via email to