Joerg,
At 07:07 AM 3/7/01 +0000, you wrote:
><snip>
>We have done some investigations on the old line standard LaB6 SRM660,
>it contains some minor phases (sum 5%), one was LaAlO3. The new
>standard SRM660a is clean and has some other advantages, too. Now,
>we favour SRM660a over Y2O3.
This is a pleasant report to hear! Will I see you at Accuracy in Powder
Diffraction III?
Best regards,
Jim
James P. Cline [EMAIL PROTECTED]
Ceramics Division Voice (301) 975 5793
National Institute of Standards and Technology FAX (301) 975 5334
100 Bureau Dr. stop 8523
Gaithersburg, MD 20899-8523 USA