Try hair spray "Clynol". You may get it in good hair cutter shops.


Viele Grüße
Wolfgang Büttner


----------------------------------------------------------------------------
----
Dr. Wolfgang Büttner
Bruker AXS GmbH
Vertrieb/Sales
Postfach/P.O.Box: 700117
D-51447 Bergisch Gladbach
Tel/Fax: +49 (0) 2202 33259
Mobile: +49 (0) 172 6870861
e-mail: mailto:[EMAIL PROTECTED]
INTERNET: http://www.bruker-axs.com
----------------------------------------------------------------------------
----


-----Original Message-----
From: [EMAIL PROTECTED] [mailto:[EMAIL PROTECTED] Behalf
Of Andreas Leineweber
Sent: Thursday, September 09, 2004 3:57 PM
To: [EMAIL PROTECTED]



Dear all,

when powder samples are measured in reflection on back-loaded samples on
a theta-2theta diffractometer, there is always the danger that upon
sample spinning the powder can fall out of its cavity. As a solution I
tried a thin mylar foil, which, however, gives nasty background. Another
procedure may be a little bit of glue (e.g. dissolved in a solvent to
dillute it).
Has somebody some practical good experiences with certain types of glues
(influence on background, how much glue, which solvent) or does somebody
know some further tricks.
Thank you for your help
Andreas

PS. I am working with the Philips/Panalytical sample preparation equipment.

--
Dr. Andreas Leineweber
Max-Planck-Institut fuer Metallforschung
Heisenbergstrasse 3
70569 Stuttgart
Germany

Telephone: +49 (0)711 689 3365
Telefax: +49 (0)711 689 3312
[EMAIL PROTECTED]
http://www.mf.mpg.de/de/abteilungen/mittemeijer/english/index_english.htm