Dear colleagues,
could anybody suggest a standard (and where i can buy), not very
expensive, like quartz or zirconia to doping a power sample to control
the position of xrd lines and probably later help in quantification.
we use Nist standard LaB6 to instrument performance characterization
Thanks a lot.