Dear members,
I'm interested in isolating the humidity parameter during one of the XRD
experiments, which seems to affect our sensitive material (some thin film on
glass).
Indeed, measuring the humidity inside the machine (SmartLab, Rigaku 3 KW)
showed quiet high humidity of 44%.
One of the options we thought about is to flow draying air into the SmartLab,
Rigaku chamber through a small aperture above the machine during the
experiments, until we reach to ~ 20% humidity.
Does the SmartLlab machine (X rays source and so on) could be damaged in such
configuration?
I guess, another option could be buying or building an appropriate sample
holder for such proposed.
Hope you can help me with that,
Thanks in advanced,
Gili
Dr. Gili Taguri,
Head of XRD lab,
Bar Ilan Institute of Nanotechnology and Advanced Materials (BINA) Bar Ilan
University
Ramat Gan 52900 Israel
lab: +972-3-7384531
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++