Joshua, You may try the COD (Crystallography Open Database) at http://www.crystallography.net/search.html where at least I was able to find an orthorhombic NbPO5 phase. Best of luck, Leo
2014-09-11 16:27 GMT-03:00 Joshua Kim <joshkim....@gmail.com>: > Dear Rietvelders, > > I am trying to do a structural refinement on a monoclinic NbPO5 powder > sample. As most of the CIF files and literature I've been able to pull up > thus far are for the orthorhombic or tetragonal phases, I am wondering if > anyone can point me in the right direction to obtaining the correct atomic > positions and lattice parameters. > > Thank You > > Josh > ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++ > Please do NOT attach files to the whole list <alan.he...@neutronoptics.com > > > Send commands to <lists...@ill.fr> eg: HELP as the subject with no body > text > The Rietveld_L list archive is on > http://www.mail-archive.com/rietveld_l@ill.fr/ > ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++ > > > -- Dr. Leopoldo Suescun Prof. Agr (Assoc. Prof.) de Física Tel: (+598) 29290705/29249859 Cryssmat-Lab./DETEMA Fax: (+598) 29241906* Facultad de Quimica, Universidad de la Republica ,_. | \ | v- ,' \ | ( \__Montevideo, Uruguay En pleno disfrute del Año Internacional de la Cristalografía 2014 ( http://www.iycr2014.org ), (http://www.cristalografia2014.fq.edu.uy)
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++ Please do NOT attach files to the whole list <alan.he...@neutronoptics.com> Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/ ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++