Your pattern match well with Bixbyite (plus some impurity)

http://www.crystallography.net/cod/9007522.html

Using FPSM

http://nanoair.dii.unitn.it:8080/sfpm/

Best

Armel


envoyé : 15 septembre 2022 à 18:37
de : KULDEEP SINGH <2019phdph...@curaj.ac.in>
à : rietveld_l@ill.fr
objet : refinement


Anybody can provide me Rietveld refinement of the following data.
angle 10-90
scane step 0.01
Pyrochlore compound 
Fe2Mn2O7


Kuldeep Singh
Research Scholar
Department of Physics
Central University of Rajasthan
Bandarsindri-305817
District-Ajmer, Rajasthan
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to