Dear Rietvelders I am attaching a zoom-in on a diffraction profile. My question is what is the origin of the step-like profile next to a very large reflection peak? Is it a sample preparation problem? Is it part of the baseline? [image: image.png] Thanks Shay --
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++ Please do NOT attach files to the whole list <alan.he...@neutronoptics.com> Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/ ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++