Hi All, I am trying to exclude the glass capillary from the weight percent calculations in my Rietveld refinement. I modeled the glass capillary using a SiO2 CIF file and made the crystallite size very small. The issue I am having now is that in the weight percent calculation it is saying the glass is ~90% of the weight. Does anyone know how I can exclude this phase from the weight percent calculation?
Thanks, Claire
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++ Please do NOT attach files to the whole list <alan.he...@neutronoptics.com> Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/ ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++