Hi there.
Have  you tried to run a analysis on the highscore plus software ?
The Highscore plus software can show the cif files which better match with
you pattern

Atenciosamente  (Yours Sincerely),
Renato B. Silva

Em qua., 23 de jul. de 2025, 10:49, Lucas Bonan Gomes <[email protected]>
escreveu:

> Dear colleagues,
>
> I'm looking for the x-ray diffraction pattern of cobalt stearate
> (C36H70CoO) at room temperature.
>
> Could someone tell me where I can find the cif file or an article that has
> this pattern? - (I couldn't find it on COD and not on ICSD either).
>
> Best regards.
> --
>
> *Dr. Lucas Bonan Gomes*
> Universidade Federal do Rio Grande do Sul
> Laboratório de Difratometria de Raios X (LDRX)
> Centro de Estudos em Petrologia e Geoquímica (CPGq/IGEO)
> (51) 3308.9924 / (51) 3308.6401
>
> Av. Bento Gonçalves, 9500
> <https://www.google.com/maps/search/Av.+Bento+Gon%C3%A7alves,+9500?entry=gmail&source=g>
> - Prédio 43126 - Sala 211
> 91501-970 - Caixa Postal 15001 - Porto Alegre / RS
>
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
> Please do NOT attach files to the whole list <[email protected]
> >
> Send commands to <[email protected]> eg: HELP as the subject with no body
> text
> The Rietveld_L list archive is on
> http://www.mail-archive.com/[email protected]/
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>
>
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to