Dear All,
Who can tell me where can I buy a zero-background quartz (or other material)
plate?
Thanks in advance for you attention
§
Natale Perchiazzi
Dipartimento di Scienze della Terra
Università degli Studi di Pisa
About zero-background quartz or silicon plates you can contact with:
"The Gem Dugout"
1652 PRINCETON DRIVE
STATE COLLEGE, PA 16803
U.S.A.
E-mail: [EMAIL PROTECTED]
Best wishes!
Vicente
Dr. Vicente José Esteve-Cano | Universitat Jaume I
[EMAIL PROTECTED] | Department of
At 12:04 19/01/99 +0100, Lubo wrote:
Hi Armel,
I am sure you will not be satisfied by this answer, but my solution to
this problem is : USE transmission geometry. We have been doing it for
years getting nice results for kaolinites, micas, vermiculites and
smectites, not to
speak of some organic