To my knowledge it is near impossible to obtain an adequate HE stain
on thick resin sections. If this is not true, I would be interested in
the same information.
Jack
On Apr 3, 2009, at 6:12 PM, Garcia, Lori, Sr. Scientist lori.gar...@medtronic.com
wrote:
This question is specifically for Linda Jenkins or anyone who has
worked
with Technovit 7200,
I am trying to do an HE stain on ~70 um thick ground sections on
plastic slides. I have followed the Donath method all the way through
processing, but the sections do not pick up stains the way the booklet
says they should. I am even having trouble following GMA staining
procedures that I have found, in fact am afraid to try too many
because
the acrylic forms tiny cracks that interfere with microscopy. I have
researched the histonet archives, but haven't found anything other
than
a couple of similar inquiries.
I would very much appreciate any advice from people who have worked
with
this specific formulation.
Happy Friday!
Lori
[CONFIDENTIALITY AND PRIVACY NOTICE]
Information transmitted by this email is proprietary to Medtronic
and is intended for use only by the individual or entity to which it
is addressed, and may contain information that is private,
privileged, confidential or exempt from disclosure under applicable
law. If you are not the intended recipient or it appears that this
mail has been forwarded to you without proper authority, you are
notified that any use or dissemination of this information in any
manner is strictly prohibited. In such cases, please delete this
mail from your records.
To view this notice in other languages you can either select the
following link or manually copy and paste the link into the address
bar of a web browser: http://emaildisclaimer.medtronic.com
___
Histonet mailing list
Histonet@lists.utsouthwestern.edu
http://lists.utsouthwestern.edu/mailman/listinfo/histonet
___
Histonet mailing list
Histonet@lists.utsouthwestern.edu
http://lists.utsouthwestern.edu/mailman/listinfo/histonet