Re: LaMnO3

2004-08-09 Thread Alan Hewat

>Has anyone a pcr file for LaMnO3 structure?

You can find LaMnO3 in the free demo ICSD database on http://icsdweb.fiz-karlsruhe.de/ 
Just choose "Details" and then "Export" the data in FullProf format.


Alan Hewat, ILL Grenoble, FRANCE  <[EMAIL PROTECTED]> fax (33) 4.76.20.76.48
(33) 4.76.20.72.13 (.26 Mme Guillermet) http://www.ill.fr/dif/AlanHewat.htm 
___



LaMnO3

2004-08-09 Thread agadis
Has anyone a pcr file for LaMnO3 structure?

Tasos Gadis
Athens University
--