In general, to push development one stop with a conventional developer, you
increase development by 1.4 times. To push two stops, you increase
development by 1.4 times twice, which is two times.
However, since pushing is really increasing the gamma rather than increasing
the film sensitivity, yo
Hello all,
I am hoping to push processing some 7266 by one stop.
Usually I develop 7266 in a lomo tank using D19 + Potassium Thiocyanate as
my first developer for 6 minutes at 20 degrees Celsius. I agitate for 10
seconds each minute.
Does anyone know how I might alter the time or temperature of