Re: cost of software.....

1999-03-11 Thread John Faber
Alan: I feel compelled to make several points in connection with the thread concerning database/software costs. As you suggested, it is important to place costs in an accurate context. A new customer license for the PDF-2 is $6,100. But this is only for the first year. ICDD produces updates e

Re: single crystal vs. powder diffraction Lattice parameter

1999-03-11 Thread Danut Dragoi
Hi, I think the difference between the lattice parameter of single crystal and powder is coming from the misoriented surface of the crystal. To detect this rotate the crystal in its own plane 360 degrees with a convenable step and plot the lattice parameter "a" versus the number of steps, you'l

Re: single crystal vs. powder diffraction Lattice parameter

1999-03-11 Thread Charles Witham
I recently encountered this with Y2O3. The literature results from single crystal measurements show a lattice parameter of 10.604 Å while powder diffraction results show 10.607 Å. I am using Y2O3 to calibrate the twotheta response of my cps-120. Originally I thought I should use 10.604 Å to cal

Re: cost of software.....

1999-03-11 Thread Armel Le Bail
Alan Hewat wrote : >I agree that the PDF is too expensive (even tho' ICDD point out that it >is only 6 cents for each of the 115,000 patterns :-) and for that reason >our lab. can't afford it either - but that's our choice too. Not a lot of compounds are synthesized at ILL, which explains that

Re: cost of software.....

1999-03-11 Thread Alan Hewat, ILL Grenoble
Ron, I suspect you are criticising the wrong people when you complain about the high cost of Oxford Cryosystems Search-Match CSM software. CSM apparently uses the ICDD powder diffraction file PDF, the product of another (American) organisation, which is indeed quite expensive. (~$6000 I b

Re: Lattice parameter of silicon in temperature

1999-03-11 Thread Dr. Jaap Vente
Patrick, Please look up the following references: J. Appl. Phys. 56(2), 15 july 1984, pp 314-320. Do note the differences that occur between cell parameters determined form single crystal and powder diffraction data. Or does anyone know of a more recent paper? regards Jaap Vente Cinvestav-IP

Lattice parameter of silicon in temperature

1999-03-11 Thread Patrick Weisbecker
Hello, Does someone has got accurate measurement of lattice parameter of Si in the range 290°K-1300°K? Thanks by advance.

cost of software.....

1999-03-11 Thread Ron Peterson
Hello everybody, In view of the recent discussion of software price I would like to add another example. Below is the exchange I had with Oxford over the price of a new search match system (as well as lots of other functions) The price is 4500 pounds with no academic( or non-commercial) price. I b