Re: checking diffractometer in capillary mode

2004-03-05 Thread zhijian fan
Sorry, this mail below should not be sent to this list. But it's very strange that it spent about eleven hours coming here. - Original Message - From: zhijian fan To: [EMAIL PROTECTED] Sent: Friday, March 05, 2004 12:51 PM Subject: Re: checking diffr

Re: CIF to powder pattern

2004-03-05 Thread Kurt Leinenweber
Hi all, With all the file converters floating around, what are the chances that we are going to proliferate files with corrupted formats? I have gotten some files already that were supposed to be "GSAS files" but didn't have 80 columns, had blank lines, etc., and I assume they were made by file c

Re: CIF to powder pattern

2004-03-05 Thread Frank, Steven
Thank you -Original Message- From: Armel Le Bail [mailto:[EMAIL PROTECTED] Sent: Friday, March 05, 2004 10:54 AM To: [EMAIL PROTECTED] Hi, >Have you had any response to your query? I also need to translate a CIF >file to hkl, d space and intensities. Thank you. No answer correspond

Re: CIF to powder pattern

2004-03-05 Thread Armel Le Bail
Hi, >Have you had any response to your query? I also need to translate a CIF >file to hkl, d space and intensities. Thank you. No answer corresponding to a complete program doing directly the job. I received advice to use XTAL : http://xtal.sourceforge.net/ or/and CIFTBX : http://www.bernstein-p

Re: Na2Ca3Al2F14 (NAC) standard

2004-03-05 Thread Anna Llobet
You will need to contact: Prof. G. Courbion [EMAIL PROTECTED] Laboratoire des Fluorures UMR6010 Faculte de Sciences et Techniques Av O. Messiaen 72085 Le Mans cedex 9 A. Llobet Magnus H. Sørby wrote: I want to purchase some standard Na2Ca3Al2F14 (NAC) powder to calibrate an Inel PSD. Does an

CIF to powder pattern

2004-03-05 Thread Frank, Steven
Dr. Le Bail, Have you had any response to your query? I also need to translate a CIF file to hkl, d space and intensities. Thank you. Steve Frank Argonne National Laboratory-West -Original Message- From: Armel Le Bail [mailto:[EMAIL PROTECTED] Sent: Friday, February 27, 2004 2:06 AM To

Magnetic Form Factor of Ru+4

2004-03-05 Thread Ozhan Unverdi
Hi All, I am doing a magnetic refinement of SrRuO3, CaRuO3, Sr(1-x)Ca(x)RuO3 and Sr2RuO4 with using FullProf. There is only Ru+1 state in the internal table of FullProf. I need to know the magnetic scattering factors of Ru+4. I will put this eight number into pcr file. Could someone give me the m

Magnetic Form Factor of Ru+4

2004-03-05 Thread Ozhan Unverdi
Hi All, I am doing a magnetic refinement of SrRuO3, CaRuO3, Sr(1-x)Ca(x)RuO3 and Sr2RuO4 with using FullProf. There is only Ru+1 state in the internal table of FullProf. I need to know the magnetic scattering factors of Ru+4. I will put this eight number into pcr file. Could someone give me the m

Re: Na2Ca3Al2F14 (NAC) standard

2004-03-05 Thread Thomas Hansen ILL
Try the CNRS lab "Laboratoire de Fluorures" at the "Université du Maine" in 72000 Le Mans, France. Armel Le Bail will know, whom to ask ;-) Thomas On 05 Mar 2004, at 14:03, Magnus H. Sørby wrote: I want to purchase some standard Na2Ca3Al2F14 (NAC) powder to calibrate an Inel PSD. Does anybody

Na2Ca3Al2F14 (NAC) standard

2004-03-05 Thread Magnus H. Sørby
I want to purchase some standard Na2Ca3Al2F14 (NAC) powder to calibrate an Inel PSD. Does anybody know where I can get it? Magnus H. Sørby Ph.D. student Institute for Energy Technology University of Oslo Dep. of Physics Dep. of Chemistry Kjeller, Norway

Re: Is it really preferred orientation problem?

2004-03-05 Thread Jon Wright
> Like Rp, Rwp, Chi2, RB are respectively from 3.96, 5.33, 2.68, 5.80 > to 3.35, 4.42, 1.85, 3.07. This should pass a test of statistical significance. That does not mean it really is preferred orientation, but if it is not preferred orientation, then you