Dear All,
if I well understood JFC correction is perfect in case of
parallel incident beam; so, in case of conventional
Bragg-Brentano diffractometer, shouldn't it work well only
in case of use of Goebel Mirrors, that get incident beam
exactly parallel?
And is it true that using Goebel Mirrors and
[EMAIL PROTECTED] wrote:
Dear All,
if I well understood JFC correction is perfect in case of
parallel incident beam; so, in case of conventional
Bragg-Brentano diffractometer, shouldn't it work well only
in case of use of Goebel Mirrors, that get incident beam
exactly parallel?
And is it true
Dear Larry,
When you removed the soller slits leading to increased the axial divergence, which profile function is appropriate to model this, especially at low angle where the asymmetry is very stark?
Kind regards
William
On 30 May 2006, at 16:01, Larry Finger wrote:
[EMAIL PROTECTED] wrote: