Re: The lower limit of crystallite size
Happy New Year to all! I think it depends of the software you are using, the analytical approach, the profile function, the number of decomposed peaks and of course - the quality of the data. I am using an old version of Topas (2.1) and according to my experience the lower limit is (with Fundamenta
The lower limit of crystallite size
Happy new year all, What is the lower limit of crystallite size that can be determined by using a bragg-brantano diffractometer? Vahit Atakan