Dear François,
Maybe you have a strongly disordered system. Depending on the type of disorder
and the distribution of diffuse intensity, it can also have an influence on the
reflection profile (thermal diffuse scattering).
Michael
Dr. Michael Wörle
Head Small Molecule Crystallography Center
Lab
Dear EXPGUI-GSAS users,
I have a problem when I try to generate a cif-file with gsas2cif:
It will just print the general positions of the space group on the screen, but
will not finish writing the cif-file.
(the last entries are the atomic coordinates of the first phase and the number
of el