Re: DBWS vs other refinement programs

2005-07-01 Thread simon billinge
OK, admission time. I put the survey together and so all boo-boos are mine. I have no affiliation with Caltech who merely host the survey. For sure I could have broken out indexing from structure solution, and probably should have. Many programs I had never even heard of, let alone used, so

RE: DBWS vs other refinement programs

2005-07-01 Thread Armel Le Bail
Are you applying ? No such ambition. Armel

RE: DBWS vs other refinement programs

2005-07-01 Thread Hewat Alan
> A lot of Rietveld programs are DBW children... More precisely Armel, a lot of Rietveld programs are children of the original Rietveld code via Harwell :-) If you actually look into the DBW code, you will seen that. Even Bob, who was at Oxford at the time, had the original code to start with, tho

Re: DBWS vs other refinement programs

2005-07-01 Thread Brian Toby
http://danse.cacr.caltech.edu/polls/results.php?sid=22 Of course, the number of people using Rietveld software is more than 269 (number of answers in the survey) The number of respondents to the survey is ~150, but Rietveld users (at least the ones who took the time to participate) on average u

RE: DBWS vs other refinement programs

2005-07-01 Thread Armel Le Bail
http://danse.cacr.caltech.edu/polls/results.php?sid=22 This Caltech survey is a bit strange. The Caltech experts range indexing programs in the category 'structure solution', mixed

RE: DBWS vs other refinement programs

2005-06-30 Thread AVDEEV, Maxim
Title: RE: DBWS vs other refinement programs Venkat, Following Vincent's reply, here is one more piece of statistics http://danse.cacr.caltech.edu/polls/results.php?sid=22 Of course, the number of people using Rietveld software is more than 269 (number of answers in the survey) and

Re: DBWS vs other refinement programs

2005-06-30 Thread Vincent Favre-Nicolin
> I have been following this mailing list for almost 2-3 > years now and I am kind of surprised to see that the > questions related DBWS program is almost nil (I did > post one question!). > > Is the DBWS's DOS interface is the main reason for,can > I say, low usage of DBWS in the refinement > comm

DBWS vs other refinement programs

2005-06-30 Thread Venkatraman S
Hello All, I use the DBWS 9411 pc program to do my refinementsI do refinements mainly to determine accurate lattice parameters and also determine subtle changes in the structure during intercalation in layered hosts etc. I have been following this mailing list for almost 2-3 years now and I a