Re: FPSM : (was Re: [EXT] [External] Re: Step-like basline)

2023-09-07 Thread Luca Lutterotti
To be more clear, they did not ask for anything except that such a paper should never be published! Luca  Luca Lutterotti Dipartimento di Ingegneria Industriale Università di Trento via Sommarive, 9 - 38123 Trento (Italy) tel. +39 0461 2824-14 (Office), -34 (X-Ray lab)

Re: FPSM : (was Re: [EXT] [External] Re: Step-like basline)

2023-09-07 Thread Luca Lutterotti
No they did not, I think the reviewer was American, in fact he was also wining about unfair competition by the EU that provides funds to develop technologies directly competing against US companies….. The FPSM was originally developed in 2013-2014 inside one EU project. I would have not develope

Re: FPSM : (was Re: [EXT] [External] Re: Step-like basline)

2023-09-07 Thread Reinhard Kleeberg
Dear Luca, the respect to your method was correctly referenced by Nicola in the Profex user manual, p. 8, since this method was (partially) implemented: https://www.profex-xrd.org/wp-content/uploads/2022/04/Profex-BGMN-Part-2-Application-EN.pdf In fact Joerg Bergmann and me have also tried simi

FPSM : (was Re: [EXT] [External] Re: Step-like basline)

2023-09-07 Thread Jonathan WRIGHT
Hi Luca, Thanks for sharing the links to your method - I hope we can try it the next time we get stuck on identification. It is a shame to hear you were delayed for so long by J.Appl.Cryst. Did they ask you to cite some work from the Glasgow group as the commercial competitor? I have in min