>I am looking for a structure for Amesite (Mg2Al)(AlSiO5(OH)4) said to be 
>C1 or P63.

There are polymorphs.  See Zheng,H. Bailey,SW. (1997) Clays & Clay Min. 45,301

BTW, this kind of question can be answered in a flash with ICSD, which every
inorganic crystallographer needs :-)  Amesite is even in the demo WWW version 
on http://barns.ill.fr/icsd which is available to all for free.

Dr Alan W. Hewat, Diffraction Group Leader, 
Institut Laue-Langevin Grenoble FRANCE <[EMAIL PROTECTED]> tel (33) 4.76.20.72.13 
ftp://ftp.ill.fr/pub/dif    fax (33) 4.76.20.76.48    http://www.ill.fr/dif/