> At 10:07 PM 3/31/98 -0500, Fred wrote:
> >>From: [email protected] (Fred Walter)
> >>Tonight I'm observing something weird. The DC amps is up to about 16,
> >>and the positive electrode seems to have an orange-colored mist coming
> >>off of it.

Y'up. That's the stuff...  Errr, how'd ya get 16 amps flowing??  
<grin>

> >I stopped the process at 25 milliamps. The water is now yellow-gold.
> >I'm not sure if I have the 'golden colloidal silver' that I hear is best,
> >or if I have something else. Any easy tests, to see if I have good stuff,
> >or a deadly poison?

Ahh, milliamps. That's better.

Everything you describe is normal for this kind of process. I was 
a little skeptical when I made my first batches, too. The biggest 
problem is the instructions people write seldom describe all the 
details of the process in excruciating detail, so there's a lot of 
room for doubt. Pictures would be nice!

You'll probably see the water darken from a tea or beer-like color, 
to more the color of amber honey over the next day or so.

If you get anything settling out over the next day or two, let us 
know. Sometimes, I think when we push the reaction for too long, we 
generate some larger particles.

On  1 Apr 98 at 4:38, Harvey wrote:
> I stop the process in thirty minutes and this is all done at room
> temperature.  The colloidal silver has a vague yellow tint to it
> after stirred/swirled and filtered.

You're probably looking at the 3-5 ppm preparations that are 
often recommended.

> When a photo or film is processed as far as you want it
> to, you put it in a fixer to stop the action of the silver and I
> don't have any clue as to what stops the action in this newly
> announced colloidal silver. 

This is an interesting comment, not as much from the subject matter,
as from its structure, intent and effect. 

Notice the entirely logical question that Harvey raises. The fact
that silver is photo-sensitive and a fixer is used in photographic
processing suggests that something must be acting as a "fixer" to
keep the HV silver preparations from being photo sensitive.

Now note that we know absolutely *nothing* about either kind of
silvers' surface properties, what kind of chemistry might be going
on, etc. Perhaps the very same process that makes golden CS quite
long lived is carried out more thoroughly in the HV process. Or any
of a million other hypotheses could be formulated.

But the effect of Henry's question is to sow doubt and even fear of
the HVAC systems. It performs the exact reverse funtion of Thomas 
Miller's comments about all the toxic yellow silver compounds in the 
Handbook of Chemistry and Physics.

Both are perfecly reasonable questions without readily available 
answers. Both raise doubts about the "other side's" product.

See how easy it is to get into pitched battles with our allies?

> When I wiped it out after it was dry, it literally silvered the
> bottom of the glass like a mirror in that one little spot.

I had the exact same happen. A simple metal cleaner, the kind you'd
use for cleaning copper bottom pans, works instantly to remove these
deposits. I bet that tomato sauce, left for a few hours, would do it
too! Someone else suggested, I think it was nitric(?) acid as
another possibility.

> A friend of mine was given a cloudy white batch of colloidal silver
> made by her nephew ... he was using sea salt as an activater and in
> my minds eye, I could just imagine all the toxins that had been
> created.

It would be straightforward to calculate the ppm concentration of 
salt used in some of these recipes. Then, if the entire quantity of 
salt turned into the most toxic silver compounds possible, figuring 
out how much you've actually made and how close that is to dangerous 
levels would be really interesting. I'd like to see this.

The other concern that Lindemann raises about the salt-assisted 
preparations is the particle size. I wonder how long her nephew's 
preparation would last before it settles out?

> He said the stuff works for him and he wasn't about to let me
> convince him otherwise.

And maybe there's nothing for us to convince him of? I use sea salt 
on my eggs in the morning. <shriek!!> 

I don't doubt that simpler is better. I hate creating unnecessary 
unknowns. But I'd like to see even a simple minded, first order, back 
of the envelope analysis that shows just what and how much serious 
toxicity one could be creating in the process.

> I spoke with Peter Lindemann this morning and he feels I am making
> it a bit strong by going 30 minutes and he recommends 20 with the
> four nine volt batteries.

I get the feeling that if I push the process for too long, I then get
the formation of some material that doesn't stay in suspension as
well. 

There is absolutely nothing wrong with using ten times as much 3-5 
ppm stuff as 30 ppm stuff! And the process for making it tends to be 
simpler.

Bottom line, I think you've got it, Fred!  Good questions Harvey!

Be well,

Mike D.

[Mike Devour, Citizen, Patriot, Libertarian]
[[email protected]                       ]
[Speaking only for myself...              ]


--
The silver-list is a moderated forum for discussion of colloidal silver.

To join or quit silver-list or silver-digest send an e-mail message to: 
[email protected]  -or-  [email protected]
with the word subscribe or unsubscribe in the subject: line.

To post, address your message to: [email protected]