--- Begin Message ---
Robert,
 I haven't been using the honey not  to speed the operation, but to
stabilize the batch. This was my understanding of what the honey was
for. My expierment wthout the honey seemed to bear this out. Can any of
you chemists out there explain what is happening? You say that using hot
water is a wives tale, but I have seen several posts saying that using
hot causes a shorter run time. What the honey ?    

--- Begin Message ---
Tom;

The first thing to do is forget the hot water and honey routine. Those are
"old wives tales."

If you want a faster start and less time then seed each new batch with about
10% of a previous batch of CS.

I have made many batches of CS as above and they do not turn yellow.  To
stop the treeing reverse the leads on the brew cell about every 10 minutes.

My newest model CS generator that I am starting to make uses 27 volts and 60
x 60 second reversal of polarity. Never clean an electrode during a run. It
also incorporates
current limiting.

You did not specify the electrode spacing. It is critical for small size and
no color.
I know what ppm I am making as I check every new set-up with my
spectrophotometer.

No color and weak Tyndall with a ppm of 10  to 15 will have very small
particle size.

The color change that you are seeing is the forming of larger particles.

If you have any questions, then answer me direct.

Robert, Ret. Elect. Engr.



--- End Message ---

--- End Message ---