Ok, I'm confused. Someone told me that you don't WANT to see your silver
wires bubbling and misting. And NOT to use saline. When I used saline, I
saw lots of mist rising off one of the wires (I'm using a small
generator with 3 9volt batteries) and the solution stayed sort of misty.
Tasted just like the gold-colored CS that I had bought from a company.
When I didn't use saline, I didn't see anything at all happening. Does
it take a lot of time? One article said DONT boil the water - another
said DO boil it. Today I heated the water to approx. 125 degrees,
started the generator and at about 11 minutes I began to see tiny
bubbles on one rod. Started timer again, and at the end of about 24
minutes the one rod was black and starting to form some deposits on the
end (but none were dropping in the water) the other rod was also
blackish and beginning to mist a bit from the end. I turned it off and
have left it alone. How do I know it's correct? Do you just assume that
you got a good solution because you had the water, silver, generator and
left it for x amount of time? I know I sound like a real dummy, but I
really want this to work for me. I appreciate all of you who have taken
time to answer me....feel free to reply to me personally if that is
best. Thanks in advance,
Pam




--
The silver-list is a moderated forum for discussion of colloidal silver.

To join or quit silver-list or silver-digest send an e-mail message to: 
[email protected]  -or-  [email protected]
with the word subscribe or unsubscribe in the SUBJECT line.

To post, address your message to: [email protected]

List maintainer: Mike Devour <[email protected]>