Hi; My name is Ron and I am new to the chat. I have been watching the list for a week or so and gathered a lot of info on cs. I received my silver electrodes yesterday and produced my first batch using 4- 9v batts. I think I got a good batch to start. Last night the batch was cloudy but this mourning it had cleared up. I had a slight yellow tint, not at all as I had expected (deeper yellow).I used 8 oz. of water electrodes were 4 '' into the distilled water for 45 min. Can anyone tell me the proper procedure using 14 Ga. wire. thanks Ron
-- The silver-list is a moderated forum for discussion of colloidal silver. To join or quit silver-list or silver-digest send an e-mail message to: silver-list-requ...@eskimo.com -or- silver-digest-requ...@eskimo.com with the word subscribe or unsubscribe in the SUBJECT line. To post, address your message to: silver-list@eskimo.com List maintainer: Mike Devour <mdev...@id.net>