Dee wrote:
Actually I would beg to differ about the plastic Marshall, as I have had negative experiences with it. I still use it, but have to 'season' the bottles first i.e. put in either distilled water or made CS and leave it for a few days. If it is made CS, it will go yellow and then I tip it away and can then use it for the next brew. This has happened with brand new PET 1 bottles. dee
I would not use PET it has plasticizers in it, which diffuse out over time. I only use HDPE, which should be completely inert. That is what the distilled water comes in, so it makes no sense to season it by putting distilled water in it, that is what the distilled water comes out of.

Marshall

Marshall Dudley wrote:
There is no problem storing CS in plastic, as long as the proper kind of plastic is used, and it is clean. 30 ppm for EIS is about the limit of what can be produced and remain stable. It is very difficult to make stable 30 ppm. Basically it has to be composed of 13 ppm of silver oxide 13 ppm of silver hydroxide, and 4 ppm of colloid. That is the saturation level of silver oxide and silver hydroxide.

Marshall




--
The Silver List is a moderated forum for discussing Colloidal Silver.

Instructions for unsubscribing are posted at: http://silverlist.org

To post, address your message to: [email protected]

Address Off-Topic messages to: [email protected]

The Silver List and Off Topic List archives are currently down...

List maintainer: Mike Devour <[email protected]>