Hi John,

Two things;

1.) Chuck the bubbler and go to mechanical stirring with a 1 1/2 v dc Radio 
shack
motor. Mechanical stirring has more action between the electrodes than does
bubbling, and makes a better product. Check the T.E.'s to see which is weaker 
for
the same brew time. Stronger the T.E. the more particles and less ionic silver
(that is what your PWT's measure).

2.) When I add H2O2 to my HVAC ARC CS that has no T.E., instantaneously there is
formed a strong T.E. which says that agglomeration has set in in a big way.

I hope this helps your understanding.

"Ole Bob"




--