OK,,so I am bit confused...but this might help separate oranges from
apples...



Subject:
          PPM ???
     Date:
          Sun, 28 Jul 2002 20:10:36 -0500
    From:
          Robert Berger <[email protected]>
 Reply-To:
          [email protected]
      To:
          [email protected], [email protected]




Hi Robb, this is "Ole Bob",
Let's try to separate the fiction from the facts about PPM. By
definition PPM is weight, BUT that is not what is measured with a PWT or

my spectrophotometer. The PWT measures the conductance of the "CS". The
spectrophotometer measures the amount of Ag+ ions which are in solution
and they(ions) will not register with a laser pointer. The laser pointer
beam reflects from colloidal particles which a metal particles, even
though in the range of 10 to 100 nm.or greater.

To find out how much total silver is in a CS brew one must have an
atomic adsorption test run to find that total silver and then a
spectrophotomet test to measure the Ag+. The difference is the amount of
Ag0 (colloids present).

In the five years that I have investigated this process I have data
logged and plotted over 300 variations of LVDC. I have made over 550 PPM
tests with my spect.

The LVDC is a very inefficient silver electroplating process, in that
the silver ions stay in solution rather than plate out on the cathode,
althought some do and appears a black sludge.

In this inefficeint process, inspite of the polarity some times some of
the Ag+ ions will agglomerate. Say if two Ag+ ions became attached to
each other the Spectophotometer and the PWT would only read it as one
ion in solution. In time they may separate into two individual ions and
would therefore measure as two ions. The total weight of silver has not
changed but what we can measure has changed.

In my earlier investigations I have found that the best indication of
the water quality is the initial current when the cell is started.

In an earlier test of two different DW; and my EZCS polarity switching
generator. the Wal-Mart DW had and initial current of
0.3 ma. The Absopure DW had an initial current of  1.7 ma. Both of these
probably would have read as zreo on a PWT.
After 2 hrs 10 min. the W-M sample measured 13 ppm and the cell current
was 3.4 ma.
The Absopure after 40 minutes sample measured 12 PPM with a cell current
of 4.6 ma.

This should tell you, if you are going to make an aqueous silver
material, you had better have a digital multimeter in the circuit.

Digging through my archives I found test run 2/8/2000 that had two
different DW's (W-M & Absopure)
#1 I1 = 0.35 ma, W-M;    #2  I2 = 1.35 ma; Absopure (I equal initial
cell current)
#1 After 2 hr &15 min. the PPM was 12.5 and I end = 3.06 ma. Total
energy input = 348 watt seconds.
#2 after 45 minutes the PPM was 13.5 and I end = 4.5 ma. Total energy
input =  244 watt seconds.
Both had no T.E. in room light, with a very faint T.E. in a darkroom.
Both of these should be called silver solutions and not silver colloids.

If you want I probably could scan this test sheet for you.

I have had 4 transmission electron microscope sample s made and two AA
samples, besides all of the spects. that I have run.

If you review the silver data that is availbe you will find that the
silver ion is what works and not the particles.

To know what you are doing takes big bucks.

It interseting that it only takes PPB (that right PPB) for silver to be
effective.

Any questions??

"Ole Bob"








--
The silver-list is a moderated forum for discussion of colloidal silver.

Instructions for unsubscribing may be found at: http://silverlist.org

To post, address your message to: [email protected]

Silver-list archive: http://escribe.com/health/thesilverlist/index.html