Trem,
Sorry, you're right, I use the gold electrode in the anode, and silver in
the black cathode...:-).  If I did as I mistyped, I'd be making CS.  I have
also experimented with both gold electrodes....it made no difference in the
final product, and with 2 gold electrodes I can make 2 batches at once.

Yes!  I use LVDC to make CG, I have the PS50 generator.  I set the current
at the highest, which is 50 - 52 volts.  I also use heated water and an
aerator pump.  I think the key is TIME.....it is a looonngg process!

Jannette


 > I'm at a loss to see how this can work.  A gold electrode just does not
> disintegrate using low voltage DC electrolysis.  At least it never has for
> me.  Gold coins lost at sea for hundreds of years come up looking the same
> as the day they were submerged and they are continually being exposed to
> electrolysis.
>
> And of course the silver electrode has to be the CATHODE (negative
polarity)
> or it will be the one to deteriorate if you use DC.  The anode is the one
> that releases particles.  Did you mistype the polarity in your post?
>
> Quite a mystery to me.  Do you know how much current is flowing?
>
> Sure you're not using their HVAC model?  Apparently it puts out 10,000 VAC
> but no current is mentioned on their website.
>



---
Outgoing mail is certified Virus Free.
Checked by AVG anti-virus system (http://www.grisoft.com).
Version: 6.0.419 / Virus Database: 235 - Release Date: 11/13/2002


--
The silver-list is a moderated forum for discussion of colloidal silver.

Instructions for unsubscribing may be found at: http://silverlist.org

To post, address your message to: [email protected]

Silver-list archive: http://escribe.com/health/thesilverlist/index.html

List maintainer: Mike Devour <[email protected]>