This problem happened to me also at one point. This was solved by
putting GSAS in the top directory. e.g. D:/GSAS
On Thu, 2 Aug 2001, Alexandros Lappas wrote:
>
>Dear All,
>
>Till recently I was using a 'no-name' Pentium II PC and Windows-98 to run routinely
>GSAS through the QBASIC interface. This was the GSAS version of 'June 2000'.
>
>Now I thought I would be better off if I would upgrade my PC and also the version of
>the GSAS!
>
>I downloaded then the 'June 2001' version of GSAS on my new HP Pentium III laptop
>running also Windows-98... and basically I can not find a way to make GSAS work!
>
>I did follow the instructions given in the 'readme' file on how to install the new
>Windows GSAS.
>However, I only managed to open the PC-GSAS interface by running the shortcut on the
>windows desktop. Anything else does not work!
>If I try to read an older gsas experiment file and then try to do 'Expedt', I never
>get that MS-DOS window that permits us to work on experiment modification. A similar
>thing happens if I try to do 'Rawplot' (in the Utilities), I never get any DOS or
>other Graphics (e.g. GrWnd) window so that I can see a plot of my data.
>
>Is there some simple solution on these problems of mine or do you think they are
>related to some kind of 'restrictions' imposed by the HP-laptop hardware?
>
>Thank you in advance.
>
>A. Lappas
>
>----------------------------------------------------------
> Dr. Alexandros Lappas
> Foundation for Research and Technology-Hellas (FORTH)
> Institute of Electronic Structure and Laser (IESL)
> P.O. Box 1527
> Vassilika Vouton
> 711 10 Heraklion, Crete
> GREECE
> Tel: +30 81 391344, Fax: +30 81 391305
> ----------------------------------------------------------
>