Then I have a "stupid question", can we replace B3+ with He with the
same number of electrons ?
Not at all! He has a much lower nuclear charge than B, so the electron
cloud of B will be much more dense at low(er) distances from the
nucleus. The corresponding atomic form factors will then decay at
markedly distinct rates with q!
Norberto
--
Norberto Masciocchi
Professor of Chemistry
Department of Science and High Technology & To.Sca.Lab.
University of Insubria
Via Valleggio, 11
22100 Como - Italy
E-mail:[email protected]
Tel: +39-031-2386613
Skype: norberto.masciocchi
Website: toscalab.uninsubria.it
******************************************
Hago cosas que me quitan un poco el mal gusto del vacío.
Y ésa es en el fondo la mejor definición del homo sapiens (J. Cortàzar)
******************************************
Justice is nothing more than the advantage of the stronger (Thrasymachus)
******************************************
Freedom is just another word for nothing is left to lose (K. Kristofferson)
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++