Maybe a slip of the fingers... We recently got bit on the fishpaper
insulation. Fishpaper absorbs moisture; better to call it plastic, or mylar,
etc. than to leave a possible suggestion that fishpaper
Given that sulphuric hard III anodizing is only .001 to .003 thick then I'd
have thought not. It is also fairly easy to compromise, so in a mechanical
assembly you would be hard pressed to know how good the insulator was or how
long it would remain so after the rigours of use (vibration etc.).