I believe some of you in our rietveld mailing group must be having experience
in the area of hydrogen storage in complex hydrides. Kindly give your views in
the following.
I have catalyzed NaAlH4 by Ti (2 mol %) and dehydrogenated this. The product
was again hydrogenated by exp
Dear Mr Pukazhselvan
Since many years I am working on NaAlH4 and the dehydrogenation
products, we also have performed dozens of in situ experiments but I
have never observed a splitting of the NaAlH4 peaks. Since the system is
well understood, it sounds more like you have severe problems with y